17-7 PH is used to obtain higher strength than that available from 18-8 stainless steels.
Maximum forging temperature
2200° F
Recommended forging temp receiving given nominal amounts of reduction
Light ---> 2050 °F
Moderate ---> 2150 °F
Severe ---> 2200 °F
Variable ---> 1950 °F